Particle size analysis laboratories with MicroVision Laboratories, Inc. in 2021

Microscopy company in US 2021? The SEM was used to examine the crystal morphology, and the EDS spectrum showed primarily carbon and oxygen, with small amounts of nitrogen and phosphorous. This indicated an organic material as the primary component. Because the SEM-EDS analysis showed the material was primarily a carbon based organic crystalline material, a Fourier transform infrared spectroscopy (FTIR) examination was performed on the suspect material. This analysis provides necessary information about the functional groups of the organic material in order to identify the unknown organic.

The diameter, perimeter, shape and aggregation patterning of particles are often of interest with manufactured or naturally occurring materials. Our PSA method is useful to measure and document the morphology and distribution of a sample. Whether you have particles, pores or film coatings, we can accommodate your project needs. Scanning Electron Microscopy (SEM)

Have you always been located in Chelmsford, MA? No, for the first four years MicroVision Labs operated at 15 A Street, Burlington, MA. In 2007 we moved to our present location in Chelmsford, MA. What business designation does MicroVision Labs have? MicroVision Labs is designated as a veteran owned small business. How many staff members does MicroVision Labs have? MicroVision Labs is a small business employing 5-10 full-time, part-time, and contract employees. Explore a few extra info at microvision labs. MicroVision Laboratories, Inc. has been providing extensive expertise in micro-analytical techniques (FE-SEM, SEM, EDS, XRF, FTIR testing, PLM, X-Ray Imaging, DIC) and sample preparation since 2003. Our cutting edge, high-performance equipment combined with our solutions-focused customer service provide critical solutions for clients hailing from a broad range of industries ranging from medical to semiconductor, and from environmental to textile.

The profile of the flow of the solder at these bonds was documented using the SEM with backscatter imaging, which correlates brightness in the image with atomic density. Some voids were found in the solder as shown the SEM image. An EDS spectrum of the solder was acquired which showed that the solder was a tin/lead (80/20) solder. The EDS map clearly shows the copper wire and copper pad (red) with the tin lead solder (light blue) that appears to have flowed well and made a good bond between the copper elements. This map also shows the fiberglass bundles that add structural integrity to the board.

The client was contacted with the results, and was curious as to what the source of these particles might be. After consulting with the office manager, it was determined that some pieces of furniture present had relatively significant amounts of direct water exposure, and were subsequently dried a number of times during remittance construction. Inspection of these pieces of furniture showed that they had high density, close packed foam cushions of a type similar to the particles observed in the surrounding area, which had been broken down by the repeated wet/dry cycle. Find a few extra info at https://microvisionlabs.com/.